Each parameter combination of temperature profile, screw configuration and screw speed leads to a specific retention time of the material in the screw barrel during processing. A color masterbatch was used to check this retention time and the time required to color the extrudate was measured. The color was added to the PLA in the main feeding section. Three measurements were carried out for each parameter setting at a material throughput of 1.5 kg/h PLA.